High temperature resistant EP conveyor belt for hot coke
Details of heat resistant EP conveyor belt :
Models:
Mode1: able to with stand the test temperature of less than 100°C, code S1
Mode2: able to with stand the test temperature of less than 125°C, code S2
Mode3: able to with stand the test temperature of less than 150°C, code S3
Mode4: able to with stand the test temperature of less than 175°C, code S4
The physical and mechanical properties of the heat resistant covering layer after tested should be in accordance with the following table:
Project | The type | ||||
T1 | T2 | T3 | T4 | ||
Change the range | |||||
Hardness | Draw the intensity | 20 | 20 | 20 | 20 |
Maximum after wearing out | 85 | ||||
Draw the intensity |
The minimum value Mpa after wearing out |
12 | 10 | 5 | 5 |
Performance rate of change /% | -25 | -30 | -40 | -40 | |
Break person who extend | Performance rate of change /% | -50 | -50 | -55 | -55 |
After aging rate of change /% | 200 | 200 | 180 | 18 |
The heat resistance conveyor belt physical property of the cover rubber after heat test shall conform to the values specified in the table:
Item | type | ||||||
type I | type II | type III | |||||
variable range | |||||||
Hardness | Difference before and after ageing (IRHD) | ±20 | |||||
Max. Value after ageing (IRHD) | 85 | ||||||
Tensile strength | variable rate in performance <= | 25 | 30 | 40 | |||
Min. value after ageing Mpa | 12 | 10 | 5 | ||||
Rate of elongation at break | variable rate in performance% <= | 50 | 55 | ||||
Min. value after ageing | 200 | 180 |
The heat resistance conveyor belt abrasive wear of the cover rubber:
Type Item level | Abrasive wear | ||
type I | type II | type III | |
First quality | 0.8 | 1 | 1 |
accepts | 1 | 1.2 | 1.2 |
The heat resistance conveyor belt layer to layer adhesion strength:
Item |
interlayer of cloth |
cover layer and cloth interlayer | |
Thickness of the cover layer ≤1.5mm |
Thickness of the cover layer >1.5mm |
||
The average value of the longitudinal specimen shall be no less than |
3 | 2.2 | 2.6 |
The peak value of the longitudinal specimen |
2 | 1.6 | 2.0 |
Our Factory RUBBER CONVEYOR BELT application in foreign countries:
Q1: What types of Conveyor Belt you can Produce?
A: Hello,Dear We can produce Sidewall,Flat,Chevron,Steel Cord Conveyor Belt,Heat Resistant,
Oil Resistant,Acid-Alkali Resistant Cold Resistant and PIPE Conveyor Belt etc.
Q2:Does your Company have ISO Certificate?
A: Yes of course we have ISO9001:2008 Certificate.
Q3:Can you Provide FORM E Certificate of Origin for us?
A: Yes we can do Normal CO,FROM E,FROM F,FORM A etc.
Q4:What is your Delivery Time?
A:Normally Within 10-20days after getting your Prepayment or L/C.
Q5:Can you give Guarantee if I buy your belt?
A:Of course,we must give Guarantee for all of our Products,Please tell me your Details of Requirement.
Q6:What is your factory's main belt?
A:Sidewall Conveyor Belt Product List for reference.
https://sidwallconveyorbelt.en.made-in-china.com/product-list-1.html.
We will be appreciated if you can provide the following specification:
1. Conveyor belt type
2. Top cover thickness
3. Bottom cover thickness
4. No.of plies
5. Width of the conveyor belt
6. Grade:
If you are not sure for any of above,we can recommend for you.
Once we get above information we will quote exact price at soonest time.